A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Re: Diffusion or Ion implantation
Re: Diffusion or Ion implantation
2003-08-06
Tiansheng Zhou
2003-08-07
Chris Kovach
2003-08-06
[email protected]
2003-08-07
Karl Cazzini
2003-08-06
Maurice Norcott
2003-08-06
[email protected]
2003-08-07
Kim Norris
Re: Diffusion or Ion implantation
Chris Kovach
2003-08-07
Diffusion or ion implantation of what?

____________________________________________
Chris Kovach, Ph.D.
Executive Director
The Center for Micro and Nano Processing
The Microfabrication Laboratory
The Electronics Design Center

Case Western Reserve University
10900 Euclid Avenue
Bingham Building, Rm 107A
Cleveland, OH,  44106-7200

Ph: (216) 368-3628
Fax: (216) 368-8738
[email protected]




-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of
Tiansheng Zhou
Sent: Wednesday, August 06, 2003 1:45 PM
To: [email protected]
Subject: [mems-talk] Re: Diffusion or Ion implantation


Hi All:

I am looking for a vendor for diffusion or Ion implantation of 4"
silicon wafers.

Thanks for any lead information.

--
Tian


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Tanner EDA by Mentor Graphics