Tanks for KOH etching
2003-08-07
Mark West
2003-08-07
beaton@npphotonics (Bill Eaton)
2003-08-07
Brubaker Chad
2003-08-11
Ertl, Stephan
Tanks for KOH etching
Ertl, Stephan
2003-08-11
Hi there !

HMR of Donaueschingen in Germany used to make a smart system with a reflow tank
made of PP. The temperature can be kept constant within less than 1°. The
company itself was sold some time ago, but people started "Lotus Systems"
(www.lotussystems.de) soon after. They should be able to provide similar
machines.

Best regards
Stephan

-----Ursprüngliche Nachricht-----
Von: beaton@npphotonics (Bill Eaton) [mailto:[email protected]]
Gesendet: Donnerstag, 7. August 2003 20:42
An: 'General MEMS discussion'
Betreff: RE: [mems-talk] Tanks for KOH etching

Food Service 304 stainless steel tanks work reasonably well. You can get
them from restaurant supply stores very easily. As an added bonus, they're
often fairly inexpensive.

Bill Eaton, Ph.D.
Materials, Analysis, and Test Manager
NP Photonics

> -----Original Message-----
> From: [email protected]
> [mailto:[email protected]]On Behalf Of
> Mark West
> Sent: Thursday, August 07, 2003 10:27 AM
> To: [email protected]
> Subject: [mems-talk] Tanks for KOH etching
>
>
> What is the preffered type of tank for KOH etching? Load is a
> single 25
> wafer cassette of 4" wafers. temp range is 80 - 100 C.
>
> Quartz is not compatible and plastic tanks are difficult to heat. Just
> wondering if anyone has found a good product for this application.
>
> M. W.
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
MEMS Technology Review
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing