CMP on SOI Substrate with buried cavities (BUCA)
2003-08-11
Marcus Siegert
2003-08-11
Renie Duvall
2003-08-11
Kenneth Smith
CMP on SOI Substrate with buried cavities (BUCA)
Kenneth Smith
2003-08-11
Renie,
Get back to me on this request. Marcus and I work together - he is in
Germany. can you quote on specification as listed ? Let me know

regards.
Ken

Renie Duvall wrote:
> Marcus,
>
> Isonics Corporation, a local SOI wafer manufacturer located in Vacouver WA not
only produces 4"-12" SOI but also offers such services as you are requesting.
Please contact Renie Duvall 360-885-9310 x 203 for further information.
>
> -------Original Message-------
> From: Marcus Siegert 
> Sent: 08/11/03 03:40 AM
> To: mems-talk 
> Subject: [mems-talk] CMP on SOI Substrate with buried cavities (BUCA)
>
>
>>Hi Colleagues:
>
> Date: 08/11/2003
>
> I need to process edge grinding, grinding and polishing (CMP) on SOI
> Substrates with buried cavities.
> Diameter of Substrates is 100 mm.
> Handle has a thickness of 525+/-15 A^?m, DSP, BOX 600+/-60 nm, with a 3 A^?m
> deep etched adjustment groove.
> Device layer has been bonded under vacuum (about 10E-3 mbar), that means
> the membran will be bowed toward inside the cavities. Device
> thickness/Initial is 300+/-15 A^?m. Final device thickness should be 50+/-0.5
A^?m, polishing
> prime with final polish because Device-Surface has to be bondable again,
> (Surface roughness <5 Angstrom).
> Struckturing of buried cavities:
> Depth: 50+/-5 A^?m
> Extensions: c. 1500 A^?m < w(Cavity) < c. 3000 A^?m
> Pitch: Deltaw (Cavity) > c. 3500 A^?m
>
> Will provide more details after contacting.
>
> Thanks and best regards,
>
> Marcus Siegert
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>
>
> 1-360-263-8011
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>


--


Kmbh Associates
47 Rocket Circle
Rancho Cordova, CA 95742  U  S  A
510-714-5055 Efax- 510 217 4421 or 561 658 6136

High Purity Float Zone and Specialty CZ Silicon  for Power, IR and
Mirror Optics, Optoelectronics, MEMS, SOI, and other Semiconductor
applications. Service in SOI, Polishing SSP and DSP.
Quartz, Glass, Pyrex and Borofloat Wafer Supply. Anodic Bonding. SOG, SOS.



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
University Wafer
The Branford Group