MEMSnet Home: MEMS-Talk: platinum wet etching
platinum wet etching
1997-10-30
Michael Koch
1997-11-06
SloanCL
platinum wet etching
Michael Koch
1997-10-30
Dear all,

is there anyone, who has worked on structuring platinum with wet
etchants? I have tried aqua-regia (3parts HCl, 1part HNO3) of 36 %,
but could not remove any Pt from my wafers. I am using ordinary
resist on top of the Pt for structuring.

Any suggestions on aqua regia or other chemicals that could etch
Pt are greatly appreciated.

Regards,

Michael
==================================================
| Michael Koch                                   |
| University of Southampton                      |
| Department of Electronics and Computer Science |
| Southampton SO17 1BJ                           |
| England                                        |
|                                                |
| Tel.: +44 (0)1703 593737                       |
| Fax.: +44 (0)1703 593029                       |
| email: [email protected]                      |
==================================================


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Mentor Graphics Corporation
Nano-Master, Inc.
MEMS Technology Review