Deposit CVD oxide on Pyrex substrate
2003-08-19
A.K.Ismail
2003-08-20
Mighty Platypus
Deposit CVD oxide on Pyrex substrate
Mighty Platypus
2003-08-20
Hey A.K.,
We haven't used pyrex, but I know that PECVD and low temperature LPCVD
oxide (LTO) both work fine on borofloat glass. I suspect pyrex will work
just as well. The only possible problem may be that the pyrex *might* not
be able to handle the temperature of LTO (about 450 C). You should have
some specififcations about the maximium temperature your glass can
withstand.

Jesse Fowler
  UCLA/MAE Dept., 420 Westwood Plaza, Room 37-129, ENGR IV
  Los Angeles, CA 90095-1597 | (310)825-3977
"Facts are stubborn, but statistics are more pliable."
   -- Mark Twain

On Tue, 19 Aug 2003, A.K.Ismail wrote:

> Dear all,
>
> Does anybody know if a low temperature CVD oxide (i.e LPCVD or PECVD) can be
> deposited on Pyrex substrate?. I would like to know if this CVD oxide can have
> a good adhesion to pyrex. I found in literature almost people deposited CVD
> oxide on Si substrate. I am expecting that it can have a good adhesion since
> pyrex is also an oxide. Could anyone who has experience about this process can
> confirm to me.
>
> Thank you.
>
> A.K.Ismail.
>
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Nano-Master, Inc.
Tanner EDA by Mentor Graphics