A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: coating on Silicon Nitride to deposit Gold
coating on Silicon Nitride to deposit Gold
2003-08-24
Nikhil Mehta
2003-08-25
Kirt & Erika Zipf-Williams
2003-08-25
Roger Shile
2003-08-26
David Ovrokzky
2003-08-25
Mahavir Sanghavi
2003-08-25
Knighton, Ed
2003-08-25
[email protected]
coating on Silicon Nitride to deposit Gold
David Ovrokzky
2003-08-26
Nick,

The simplest way to deposit Gold in your case is as follows:
1. Sputtering of Ni/V7% (very often used target) on Silicon Nitride.
2. Plating of Electroless Ni (mid or high phosphor, for example from ENTHONE
company).
3. Plating of immersion or electroless Gold (also from ENTHONE or Akuno).

All these metal layers are not sensitive to KOH.

Also, you can perform lithography of Ni/V7% using AZ resist and TRANSENE
etchant

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of
Nikhil Mehta
Sent: Sunday, August 24, 2003 10:30 PM
To: [email protected]
Subject: [mems-talk] coating on Silicon Nitride to deposit Gold


hi:
We at present are do a titanium coating on Silicon Nitride on which we
deposit Gold (as gold does not stick to Nitride). I am looking for
literature to find if we can replace titanium with any other material on
which we can deposit Gold and at the same time this material is not
sensitive to KOH etching (Titanium is sensitive to KOH etching).

I tried to find some literature on this but no success. Can any one help me
in my dilemma

thanks

Nick
Graduate Student
Auburn University



---------------------------------
Do you Yahoo!?
Yahoo! SiteBuilder - Free, easy-to-use web site design software
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMS Technology Review
Addison Engineering
Process Variations in Microsystems Manufacturing