mems work
2003-08-11
Andreas Scheipers
2003-08-11
Brubaker Chad
2003-08-13
Tom Fan
2003-08-13
Ji'e (Jayne) Wu
2003-08-18
Andreas Scheipers
2003-08-18
Jochen Zöllin
2003-08-25
Andreas Scheipers
2003-08-13
Brubaker Chad
2003-08-26
Randy Grow
2003-08-26
Michael D Martin
2003-08-26
Brubaker Chad
Electrodes in Microchannel
Brubaker Chad
2003-08-26
Randy,

The spay coating process mentioned previously (ultrasonic, by EVG, rather than
electro-spray) has been used to successfully conformally coat with PMMA. Other
than that, I'm not sure as to an effective method to produce the thin film you
are looking for in a conformal coat.

Best Regards,

Chad Brubaker

EV Group       invent * innovate * implement
Technology - Tel: (602) 437-9492, Fax: (602)437-9435 e-mail:
[email protected], www.EVGroup.com

This message and any attachments contain confidential or privileged information,
which is intended for the named addressee(s) only. If you have received it in
error, please notify the sender immediately and then delete this e-mail. Please
note that unauthorized review, copying, disclosing, distributing or otherwise
making use of the information is strictly prohibited.


 -----Original Message-----
From:   Randy Grow [mailto:[email protected]]
Sent:   Tuesday, August 26, 2003 8:41 AM
To:     [email protected]
Subject:        Re: [mems-talk] Electrodes in Microchannel

Does anyone have a recommendation for a conformal layer of PMMA? I have
8 micron steps that have been difficult to cover. I have succeeded with
a  bilayer of PMMA, each layer being 1.6 microns, for a total of 3.2
microns. At that thickness, though, ebeam lithography becomes very
difficult.

Thanks,

Randy Grow
Ph.D. Candidate
Dept. of Applied Physics
Stanford University


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
The Branford Group