Hello Everybody


!
    Please help in following regards



    1) I would like to know the process parameters(temperature and
concentration of etchants) and the etchants required for etching 500 micron
hole through normal glass and pyrex 7740. The masking layer will be
Cr/AU.
    2) Vendors for pyrex 7740, who can deliver some 30 pieces of pyrex
7740 at earliest. I'm based in India.
    3) The kind of (quality and quantity) of work I should do on anodic
bonding and glass etching to get an IEEE paper published



    Thanking in advance to those who reply.



    with warm regards to all



    BALGOVIND
Get Your Private, Free E-mail from Indiatimes at  http://email.indiatimes.com
Buy The Best In BOOKS at http://www.bestsellers.indiatimes.com
Bid for Air Tickets on Air Sahara Flights at Prices Lower Than Before. Just log
on to http://airsahara.indiatimes.com and Bid Now !
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Addison Engineering
Tanner EDA by Mentor Graphics