2003-09-06
GuyHaché
2003-09-07
Christopher Blanford
how to buy a CO2 supercritical dryer
GuyHaché
2003-09-06
Hi,

I am searching for some information about CO2 supercritical dryer.  I would like
some suggestions about which compagny I should approach to buy a CO2
supercritical dryer or which I should not! If you also know some publications
that cited  a particular CO2 supercritical dryer or if you use (or sell) one,
please contact me.

Thank's,


Guy Haché, M.Sc.A.
Assistant de recherche, research assistant
--------------------------------------------------------
Département de génie électrique et de génie informatique
Université de Sherbrooke
2500, boulevard Université
Sherbrooke (Québec) Canada
J1K 2R1
Téléphone/phone : (819) 821-8000 3706
Télécopieur/fax : (819) 821-7937
e-mail: [email protected]
--------------------------------------------------------




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
University Wafer
Process Variations in Microsystems Manufacturing