BCB adhesive wafer bonding
Richard Jiang
2003-09-14
Hi all,

I am interested in MEMS wafer bonding using dry etch BCB or photo-BCB from DOW
Chemicals. Does anyone can tell me which BCB, dry etch BCB or photo-BCB, is more
easier to perform adhesive wafer bonding successfully?

I want to bond a MEMS device and a silicon cap (with cavities etched in it)
together.

Best regards,

Richard Jiang


=====
Richard Jiang

Shanghai Institute of Microsystem and Information Technology, CAS
865 Changning Road
Shanghai 200050, China
[email protected]
Tel: 86-21-62511070-5966

__________________________________
Do you Yahoo!?
Yahoo! SiteBuilder - Free, easy-to-use web site design software
http://sitebuilder.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Nano-Master, Inc.