To: Jan Kowal
From: KlemicJ on Thu, Feb 6, 1997 5:29 PM
Subject: RE: Ultrasonic drilling

Jan Kowal,
    I have drilled many holes in silicon and glass in the 250 to 750 micro
meter range. I do not use ultrasonic methods, simply a diamond drill in a
specialized set up on a good milling machine. If you know how to uudecode (or
whatever your preference) I can e-mail you pictures, or if you have a
disposable sample, I can drill some sample holes for you and let you know how
much it would cost to do what you want.
     John Klemic
     Biology Shop
     Caltech 156-29
     Pasadena, CA 91125
     USA
Phone: 818-395-8491
   fax: 818-449-0756
_______________________________________________________________________________
To: [email protected]
From: Jan Kowal on Thu, Feb 6, 1997 5:16 PM
Subject: Ultrasonic drilling
RFC Header:Received: by starbase1.caltech.edu with SMTP;6 Feb 1997 17:16:06
-0800
Received: by darkstar.isi.edu (5.65c/5.61+local-24)
        id ; Thu, 6 Feb 1997 16:06:19 -0800
Received: from venera.isi.edu by darkstar.isi.edu (5.65c/5.61+local-24)
        id ; Thu, 6 Feb 1997 16:06:08 -0800
Received: from darkstar.isi.edu by venera.isi.edu (5.65c/5.61+local-26)
        id ; Thu, 6 Feb 1997 16:06:06 -0800
Received: by darkstar.isi.edu (5.65c/5.61+local-24)
        id ; Thu, 6 Feb 1997 16:06:06 -0800
Message-Id: <[email protected]>
Reply-To: Jan Kowal 
Date: Thu, 06 Feb 1997 16:26:34
Subject: Ultrasonic drilling
From: Jan Kowal 
To: [email protected]
X-Url: http://mems.isi.edu/mems.html

Does anyone know where I can get ultrasonic machining of glass and
silicon done?  Typically, I need large numbers of holes in the
sub-millimetre range drilled into 3" and 4" substrates, up to 1mm
thick.

--
Jan Kowal
Applied Microengineering Ltd
68 Milton Park
Abingdon, Oxfordshire, UK
Tel: +44 (0)1235 833934
Fax:             833935
e-mail: [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Addison Engineering