ZnO etching
1997-11-15
Matjaz Valant
ZnO etching
Matjaz Valant
1997-11-15
You Can use a distilled water with a few drops of concentrated HCL for a
10 seconds.

Could you answer me, where can I find what happened with ZnO in water,
why the pH value do not become stable and how can I fix the pH value for
zeta potential meausurment?

Thank You. Andrej Degen. ([email protected])