Protective Coating in KOH solution!!!!
2003-11-07
KANISHKA BISWAS
RE : [mems-talk] Protective Coating in KOH solution!!!!
2003-11-07
Christophe Gorecki
2003-11-07
Shane Jones
2003-11-07
Zhang, Wenyue(Lydia)
2003-11-12
Neal Ricks
2003-11-14
Glenn Silveira
2003-11-07
Michael L
2003-11-14
Kretschmer Hans-Richard
Protective Coating in KOH solution!!!!
Neal Ricks
2003-11-12
Hello,
I have heard of people using Shipley BPR100 for this application, although I
myself, have not.  You may contact Bob Forman at [email protected] for more
information.

Neal Ricks
Wafer Fab Manager
Shipley Co., LLC
EIF Division

KANISHKA BISWAS  wrote:
Hi Everybody,
Can any one suggest a protective coating (polymer etc)for protecting the top
surface of silicon wafer with aluminium lines while etching the back side of the
wafer using KOH solution???? We have already tried out wax, black wax coatings
but it did not work.
Any help and references in this regard will be highly appreciated....
Thanks
Kanishka


____________________________________________________________
FREE ADHD DVD or CD-Rom (your choice) - click here!
http://ad.doubleclick.net/clk;6413623;3807821;f?http://mocda2.com/1/c/563632/131
726/311392/311392
AOL users go here: http://ad.doubleclick.net/clk;6413623;3807821;f?http://mocda2
.com/1/c/563632/131726/311392/311392
This offer applies to U.S. Residents Only

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

---------------------------------
Do you Yahoo!?
Protect your identity with Yahoo! Mail AddressGuard
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
University Wafer
Harrick Plasma, Inc.