A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: zinc oxide ZnO and metals
zinc oxide ZnO and metals
2003-11-18
Steven F. Nagle
2003-11-18
Shweta Humad
2003-11-19
Jim Intrater
2003-11-19
Steven F. Nagle
zinc oxide ZnO and metals
Shweta Humad
2003-11-18
I use Aluminum on ZnO and it adheres well. I don't need a Pt layer for
adhesion to Al.
Havent tried any other metals though.

--
Shweta Humad


-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf
Of Steven F. Nagle
Sent: Monday, November 17, 2003 9:04 PM
To: [email protected]
Subject: [mems-talk] zinc oxide ZnO and metals


Can anyone tell me several metals that adhere well to zinc oxide?  More
specifically, would we need an adhesion layer for Pt?

Thanks.



_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
MEMS Technology Review
University Wafer