MEMSnet Home: MEMS-Talk: via through pyrex
via through pyrex
2003-12-15
Paolo Bondavalli
2003-12-17
David Nemeth
2003-12-17
Steven F. Nagle
2003-12-17
Choe,S-H
2003-12-16
[email protected]
via through pyrex
[email protected]
2003-12-16
This is a particularly difficult process. I have tried a variety of high power
rie processes using SF6 NF3 Chlorine BCL3 with poor results. It would seem to me
that due to the composition of the material ie inclusion of AL2O3 in the pyrex
negates the ability to make  compounds that can be plasma etched away. Bob
Henderson


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Addison Engineering
University Wafer
Process Variations in Microsystems Manufacturing