Wong
2003-12-23
Yes i have sputtering experience using copper for pyrex glass 7740. By the way
do u have any jobs for a post of semiconductor engineering in singapore? Looking
forward to hear from you. Thanks

________________________________

From: [email protected] on behalf of
Dipankar Ghosh
Sent: Tue 12/23/2003 2:41 AM
To: General MEMS discussion
Subject: [mems-talk] Sputtering of copper




Hi all,
       I would like to sputter Cu (thickness of about 2 microns) . However i
understand that i need to modify my sputtering parameters to do this.

Currently my parameters are :-

Pr(base)= 5 * 10 ^(-5) torr

Pr (chamber)= 30 m torr

Power = 300 W



Does anybody have any experience in sputtering thick Copper.Pls let me know.

Thanks in advance,
             Dipankar Ghosh





____________________________________________________________
Free Poetry Contest. Win $10,000. Submit your poem @ Poetry.com!
http://ad.doubleclick.net/clk;6750922;3807821;l?http://www.poetry.com/contest/co
ntest.asp?Suite=A59101

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
Mentor Graphics Corporation
Nano-Master, Inc.