MEMSnet Home: MEMS-Talk: hard bake before HF
hard bake before HF
2004-01-06
[email protected]
2004-01-07
R. Brent Garber (2 parts)
2004-01-06
[email protected]
2004-01-08
[email protected]
2004-01-09
Eric TANG Xiaosong
hard bake before HF
R. Brent Garber
2004-01-07
Rajan,

In most cases you can hard bake resist for hours and HF will still under
cut.  Cr masks are used more often for a HF mask.

Brent

[email protected] wrote:

> hi all
> can anyone plsease telll me what should be the ideal post bake(hard bake)
> before HF
> etching of silicon iam using PR-SR1813.
> regards
>
> Rajan Malik
> Graduate Student
> Electrical Engg.
> University of south Florida
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
garber.vcf (text/x-vcard, 361 bytes)
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Addison Engineering
Tanner EDA by Mentor Graphics