MEMSnet Home: MEMS-Talk: Kapton Sputtering
Kapton Sputtering
1997-12-23
Michael Young
Kapton Sputtering
Michael Young
1997-12-23
Does anybody have experience with sputtering metal film on Kapton
sheet?  We are experiencing problems with Kapton curling and film
cracking.  Any suggestions?

--
Michael Young
ACSI
18 Technology Drive, Suite 139
Irvine, CA 92618
TEL (714)453-8988   FAX (714)453-8987
E-mail: [email protected]
Web site: http://www.acsensor.com/