How to fabricate Via holes through pyrex glass
2004-01-15
Eva Piñar
How to fabricate Via holes through pyrex glass
Eva Piñar
2004-01-15
Hi!

I am designing a structure for a microfluidic application, and i am thinking
about the possibility of bonding (anodic bonding) a pyrex glass with a silicon
structure.

I would need to open a through-wafer via in pyrex (20 um diameter), and i would
like to know if this is possible. I have read in a message that maybe
photosensitive glass would be more suitable for this.

I would like to know if any machinig (in fact, opening the via) can be done
after bonding, without any damage to de device.

Thanks everybody, Eva.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMS Technology Review
The Branford Group
Nano-Master, Inc.