Ask for dry etching machine that can do soda lime glass etching?
2004-01-15
[email protected]
Ask for dry etching machine that can do soda limeglass etching?
2004-01-16
mizur
Ask for dry etching machine that can do sodalimeglass etching?
2004-01-16
Kirt Williams
Ask for dry etching machine that can do soda limeglass etching?
mizur
2004-01-16
I think quartz etches pretty well. The aditives in the glass / pyrex kill
the process. I think the chemistry is as a chalange as the hardware.
Shay
----- Original Message -----
From: 
To: "General MEMS discussion" 
Sent: Friday, January 16, 2004 1:54 AM
Subject: Re: [mems-talk] Ask for dry etching machine that can do soda
limeglass etching?


> This sounds like a great challange for the MEMS community. Why don't we
try to get a forum together to discuss ideas on how to dry etch pyrex,soda
lime glass, quartz ect. Let's try something like "The ideal dry etch tool
for etching pyrex ect would have the following hardware/process features."
>
> I would submit that the system must have an electrostatic helium backside
clamp capable of holding glass wafer with backside pressure of say 20 torr
and a gas flow of <1sccm
> Bob Henderson
>
> Next?????????
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering
Harrick Plasma, Inc.