Aging of sputtered chrome
2004-01-14
Mister Einstein
2004-01-18
Jim Intrater
Aging of sputtered chrome
Jim Intrater
2004-01-18
It adsorbs species (e. g., O2) from the air which in turn increases the
surface tension of water on it. The fresh layer of pure Cr will induce
aggressive wetting.

-Jim Intrater

----- Original Message -----
From: "Mister Einstein" 
To: 
Sent: Wednesday, January 14, 2004 2:12 PM
Subject: [mems-talk] Aging of sputtered chrome


> Does anyone know why a surface sputtered with chrome
> would become more hydrophobic over time?  I can
> accelerated the process by baking at 85C for a minimum
> of 12 hours and I can reverse the process using 1N HCl
> or NaOH.  Any explanations are appreciated
>
> __________________________________
> Do you Yahoo!?
> Yahoo! Hotjobs: Enter the "Signing Bonus" Sweepstakes
> http://hotjobs.sweepstakes.yahoo.com/signingbonus
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
MEMS Technology Review
Tanner EDA by Mentor Graphics