MEMSnet Home: MEMS-Talk: wafer and glass for SOG
wafer and glass for SOG
2004-01-20
Lee, Duhyun
2004-01-21
Carsten Wesselkamp
wafer and glass for SOG
Lee, Duhyun
2004-01-20
Dear MEMS-talkers,
I'm trying to make SOG wafer by anodic bonding and CMP.
Could you recommend me the Si wafer and glass for it?

I want to know the followings;
 - kind of glass - I'm gonna try corning 7059 or 1737F.
 - thickness of glass and Si wafer
 - TTV level of Si wafer and glass
 - other factors I should consider

Thank you

Lee, Duhyun

========================================
[email protected]
Technology Innovation Center(TIC)
Dep. of Advanced Materials Eng.
Sungkyunkwan University, KOREA
Tel +82-31-290-5645
Fax +82-31-290-5644
========================================
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
The Branford Group
University Wafer