MEMSnet Home: MEMS-Talk: Reflectivity vs Coated Aluminum Thickness
Reflectivity vs Coated Aluminum Thickness
2004-01-08
Kimi
2004-01-23
Kimi
2004-01-24
David Grove
2004-01-24
Nels P Ostrom
Reflectivity vs Coated Aluminum Thickness
David Grove
2004-01-24
At the link below you find a model of Al reflectance vs. thickness on Si
(100 microns) using film star. The three lines are 600, 700, and 800 nm from
top to bottom. The second graph is the same model with Ag for comparison.
The third is reflectance vs. wavelength for Ag and Al, notice the dip in the
Al due to Al's absorptance peak at 800nm. You need very little Al to reach
your peak reflectance, the curve is basically flat from this point on. These
were modeled using Filmstar.



http://www.rockisland.com/~dgrove/images/Reflectance.doc



Hope this helps,





David Grove

Chief Research Engineer

www.luxel.com



A good politician is like a good football coach. He must be smart enough to
do a good job but dumb enough to think it matters...




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Harrick Plasma, Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics