MEMSnet Home: MEMS-Talk: si etch with tmah, type N or P
si etch with tmah, type N or P
2004-01-30
GuyHaché
2004-01-31
Kirt Williams
si etch with tmah, type N or P
GuyHaché
2004-01-30
Hi,

When using TMAH to etch Si, is it better to use type N or type P Si for a high
etch rate?

Is it better heavily doped or lightly doped?

Thank's


Guy Haché, M.Sc.A.
Assistant de recherche, research assistant
--------------------------------------------------------
Département de génie électrique et de génie informatique
Université de Sherbrooke
2500, boulevard Université
Sherbrooke (Québec) Canada
J1K 2R1
Téléphone/phone : (819) 821-8000 3706
Télécopieur/fax : (819) 821-7937
e-mail: [email protected]
--------------------------------------------------------

--------------------------------------------------------------------------------





reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Nano-Master, Inc.
Addison Engineering
Process Variations in Microsystems Manufacturing