SU-8 can resist Cu electrolyte?
[email protected]
2004-02-01
Yes, it can. Check also with Mark Shaw ([email protected]).

----- Original Message -----
From: "Lee, Duhyun" 
To: 
Sent: Wednesday, January 28, 2004 6:59 PM
Subject: [mems-talk] SU-8 can resist Cu electrolyte?


> Dear MEMS talkers,
>
> I'm trying to use SU-8 to mask a wafer during eletroplating the Cu and
Tin.
> I want to know whether the SU-8 can resist above electrolytes?
>
> Lee, Duhyun
>
> ========================================
> [email protected]
> Technology Innovation Center(TIC)
> Dep. of Advanced Materials Eng.
> Sungkyunkwan University, KOREA
> Tel +82-31-290-5645
> Fax +82-31-290-5644
> ========================================
>
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/






reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.