MEMSnet Home: MEMS-Talk: TMAH Resistant Coating
TMAH Resistant Coating
2004-02-02
Preston Larson
2004-02-03
Mark Fuller
2004-02-17
Russell Davies
TMAH Resistant Coating
Preston Larson
2004-02-02
Dear MEMS experts,

I am searching for some type of organic coating that can be spun on or
brushed on that is insoluble in TMAH at 85°C.  Possibly something that
is somewhat similar to a photoresist that can also be removed easily
after the TMAH etch has been completed.  I am seeking to use this as a
protective mask as opposed to using an oxide mask.  Any suggestions that
you can provide would be greatly appreciated.



Preston Larson
Graduate Research Assistant
University of Oklahoma
Dept. of Physics and Astronomy
440 W. Brooks Street
Norman, OK 73019





reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
University Wafer
Process Variations in Microsystems Manufacturing
MEMStaff Inc.