MEMSnet Home: MEMS-Talk: Looking for Au sputtering sub-contractor
Looking for Au sputtering sub-contractor
2004-02-03
Albrecht Andreas
Looking for Au sputtering sub-contractor
Albrecht Andreas
2004-02-03
Dear colleagues,
at this time we are looking for a service contractor for doing backside
sputtering gold on 4" Si wafers.
The lot comprises 500 wafers. Could anyone help?
Please send your answer emails only directly to my personal email
address [email protected] and NOT to the mailing list.

Regards

Andreas Albrecht
CiS Institut fuer Mikrosensorik gGmbH
Konrad-Zuse-Str. 14
99099 ERFURT

Tel. +49-361-6631475
Fax +49-361-6631423
URL: http://www.cismst.de
Email: [email protected]



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMStaff Inc.
MEMS Technology Review
The Branford Group