MEMSnet Home: MEMS-Talk: What could be wafer surface temperature during sputter deposition w/ Al deposition, 10000W, 150sccm Ar flow, 12min deposition time?
What could be wafer surface temperature during sputter deposition w/ Al deposition, 10000W, 150sccm Ar flow, 12min deposition time?
2004-02-05
Cheol Han
What could be wafer surface temperature during sputter deposition w/ Al deposition, 10000W, 150sccm Ar flow, 12min deposition time?
Cheol Han
2004-02-05
Could anybody comment what could be the wafer surface temperature during
following sputter deposition?
Al deposition, 10000W, 150sccm Ar flow, 12min deposition time
Any comments should be appreciated. Regards,
Cheol Han
Sr. Packaging Engineer
Packaging Technology Group
National Semiconductor
3707 Tahoe Way
Mail Stop 19-100
Santa Clara, CA 95052-8090
Tel: 408-721-7362
Fax: 408-746-2007
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics