A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Si and glass wafer spec. for SOG bonding
Si and glass wafer spec. for SOG bonding
2004-02-09
Lee, Duhyun
Si and glass wafer spec. for SOG bonding
Lee, Duhyun
2004-02-09
Dear MEMS talkers,

Please advice me what kind of wafer spec. I have to consider to make SOG
wafer.
I'm going to use andic bonding process to bond a  Si and glass.

What is the conventional spec. for following terms?
- Roughness of Si and glass
- Thickness of Si and glass
- Resistivity, doping type, and cryatalline plane of Si wafer
- Kind of glass

Thank you

Lee, Duhyun

========================================
[email protected]
Technology Innovation Center(TIC)
Dep. of Advanced Materials Eng.
Sungkyunkwan University, KOREA
Tel +82-31-290-5645
Fax +82-31-290-5644
========================================




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Harrick Plasma, Inc.
The Branford Group
Process Variations in Microsystems Manufacturing