MEMSnet Home: MEMS-Talk: Conductive substrates for processing SU-8
Conductive substrates for processing SU-8
2004-02-11
Mark Leonard
2004-02-12
Edward Blackwell
2004-02-11
Michael D Martin
2004-02-11
[email protected]
Conductive substrates for processing SU-8
[email protected]
2004-02-11
Hi Mark,

 You can use a mirror finished nickel substrate. But I believe you will have
to spend some time in optimizing the SU 8 process on a nickel substrate. But
the time spent on polishing a nickel substrate I guess, would pretty match
equal the time for depositing your metal seed layer. If processing time is
all that you are concerned about, then the ideal thing is to obtain polished
nickel substrates.

Sreeram

-----Original Message-----
From: Mark Leonard [mailto:[email protected]]
Sent: Wednesday, February 11, 2004 3:59 AM
To: [email protected]
Subject: [mems-talk] Conductive substrates for processing SU-8


Hello all,

I am currently using the UV-LIGA process with SU-8 to fabricate metallic
MEMS devices as part of my PhD work. Since my devices are removed from the
substrate after fabrication I use the cheapest wafers possible, onto which I
deposit a conductive seed layer by chemical vapour deposition to form a
plating base. I was wondering if anyone has experience using a suitable
conductive substrate which cuts out the need to deposit the conductive seed
layer and hence save on processing time. I have noticed that SU-8 does not
adhere well to some surfaces such as copper. I have also noticed that
substrates which do not have a mirror finish result in poor quality
features, presumably because of scattering. It would be much appreciated if
anyone has any suggestions on potential conductive substrates that I can try
for my process.


Mark
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

----------------------------------------------------------------------------
----------------- CONFIDENTIAL AND PRIVILEGED INFORMATION ------------------

This email, including attachments, contains information that is privileged,
confidential or subject to non-disclosure agreements or intellectual
property laws.  This email, including attachments, constitutes non-public
information intended to be conveyed only to the designated recipient(s).  If
you are not the intended recipient, please delete this email, including
attachments, and notify the sender by return mail, email, or by calling (ALL
CONTACT INFORMATION LISTED BELOW). The unauthorized review, use,
dissemination, distribution, or reproduction of this email, including
attachments, is prohibited and may be unlawful.

APPLIED IMAGE Group / Optics subsidiary
4400 South Santa Rita Avenue
Tucson, AZ 85704
phone:  520-806-3800
fax:    520-806-3899

----------------- CONFIDENTIAL AND PRIVILEGED INFORMATION ------------------
----------------------------------------------------------------------------



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Harrick Plasma, Inc.
University Wafer