A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: thick photoresist development
thick photoresist development
2004-02-16
Qing Yao
2004-02-16
Isaac Wing Tak Chan
2004-02-16
[email protected]
2004-02-16
[email protected]
2004-02-17
Gary
2004-02-17
Brubaker Chad
2004-02-17
Kevin
2004-02-18
Brubaker Chad
2004-02-18
Bill Moffat
thick photoresist development
[email protected]
2004-02-16
Qing:

I don't think you will ever get the results you are looking to make with the
process you described. Contact the photoresist manufacturer first for
suggestions on how to do multiple coats of resist. You might need to bake for a
longer time at a lower temperature to begin with. Your exposure method is also
suspect. I am sure someone within the MEMS community has the proper equipment
for exposure you might be able to borrow or even do a joint development project
with to help you along. Bob Henderson


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Harrick Plasma, Inc.
Mentor Graphics Corporation
University Wafer