GuyHaché
2004-02-18
Philip Lau
2004-02-18
[email protected]
tmah solution: refresh and nickel
Philip Lau
2004-02-18
Nickel in TMAH
*************

Guy,
    TMAH, because of its caustic nature will attack Aluminium (Nickel?), but
Aluminium erosion can be slowed down (mitigated) if you mix TMAH with a
certain amount of Silicon fragment additives [scavenger].

Nickel, I do not know. You will have to do some nickel etchrate experiments
and/ XPS to see the amount of oxidation.

Phil

----- Original Message -----
From: "Guy Haché" 
To: 
Sent: Tuesday, February 17, 2004 10:27 PM
Subject: [mems-talk] tmah solution: refresh and nickel


> Hi,
>
> I have achieved a 45 microns/hour Si etch rate with TMAH (thank's to all
your
> answers).
>
> In order to keep an etch rate over 30 microns/hour, when should I do
another
> TMAH solution?
>
> I would also like to know if the TMAH attacks Nickel?
>
> Thank's
>
>
> Guy Haché, M.Sc.A.
> Assistant de recherche, research assistant
> --------------------------------------------------------
> Département de génie électrique et de génie informatique
> Université de Sherbrooke
> 2500, boulevard Université
> Sherbrooke (Québec) Canada
> J1K 2R1
> Téléphone/phone : (819) 821-8000 3706
> Télécopieur/fax : (819) 821-7937
> e-mail: [email protected]
> --------------------------------------------------------
>
> --------------------------------------------------------------------------
------
>
>
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMStaff Inc.
Nano-Master, Inc.
Mentor Graphics Corporation