A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Alumina safe isotropic Silicon etchant
Alumina safe isotropic Silicon etchant
2004-02-18
Tripp, Marie Kathleen
2004-02-18
William Lanford-Crick
2004-02-19
Cyrille Hibert
2004-02-18
Fabio Tagliareni
2004-02-18
Michael Marrs
Pt1000 RTD......
2004-02-19
Kamal Kishore
Alumina safe isotropic Silicon etchant
Fabio Tagliareni
2004-02-18
Hi Marie,

I think you can use also RIE (dry etch) for etching Silicon. I have used a
SF6, CHF3, O2 chemistry for etching Si with about 1 µm/min. Aluminium ist
not etched in my case but I don't know exactly about AlO or Al2O3.


Regards

Fabio Tagliareni


-----Ursprüngliche Nachricht-----
Von: [email protected]
[mailto:[email protected]]Im
Auftrag von Tripp, Marie Kathleen
Gesendet: Mittwoch, 18. Februar 2004 15:45
An: [email protected]
Betreff: [mems-talk] Alumina safe isotropic Silicon etchant


Hello,  I am looking for an etchant (either wet or dry) that will isotropic
etch Silicon but not affect Alumina (Al22O3, Alumina Oxide).  Can anyone
recommend anything other than XeF2?  Thanks, Marie

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing