problem with polyimide ashing
ASIC Hello
2004-02-19
Hi all,

I am trying to ash polyimide PI2610 patterns using
Plasma-finish asher. My polyimide patterns are 50 um x
50 um and about 2.2 um thick. Masking layer for
polyimide is SiNx layer. However ashing process seems
to be slow (60 ~ 90 minutes). My recipe is:

O2 400 sccm
N2 50 sccm
Pressure 200 Pa
Power 400 W .

In additionally, thin film of 1200 A of gold beneath
PI2610 is etched. There is black residue on gold film.

Could anyone advice me a better PI ashing recipe,
which can prevent gold layer and ash PI2610 faster?

Thank in advance

Chi Anh

__________________________________
Do you Yahoo!?
Yahoo! Mail SpamGuard - Read only the mail you want.
http://antispam.yahoo.com/tools


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Mentor Graphics Corporation
Nano-Master, Inc.