Hello Pankaj,

You did not mention the method of deposition. Are you using thermal
evaporator, sputtering, e-beam. How thick is your polymer.?


Aasutosh Dave


>From: Pankaj Kaul 
>Reply-To: [email protected], General MEMS discussion
>
>To: [email protected]
>Subject: [mems-talk] metal deposition on polymer/ aerogel
>Date: Thu, 19 Feb 2004 12:09:25 -0500
>
>Hi all,
>
>I'm facing problems in depositing Al 200nm or Au 200nm on Polymers and
>Aerogel samples.
>
>Can any anybody suggest me any technique / method for doing that.
>
>Thanks,
>Pankaj Kaul
>
>
>Department of Mechanical & Aerospace Engg
>Case Western Reserve University
>Euclid Avenue , Cleveland.
>
>
>
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/

_________________________________________________________________
Get fast, reliable access with MSN 9 Dial-up. Click here for Special Offer!
http://click.atdmt.com/AVE/go/onm00200361ave/direct/01/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
University Wafer
Process Variations in Microsystems Manufacturing
MEMStaff Inc.