MEMSnet Home: MEMS-Talk: RE: [email protected] - Email found in subject - [mems-talk] ITO Etch selective to glass
RE: [email protected] - Email found in subject - [mems-talk] ITO Etch selective to glass
2004-02-23
Borski, Justin
Coating of hydrophobic polymer surface
2004-02-24
Kristjan Leosson
Surface tension on inclined rigid walls
2004-02-24
Alejandro Allievi
RE: [email protected] - Email found in subject - [mems-talk] ITO Etch selective to glass
Borski, Justin
2004-02-23
Hi Anthony,

17% HCL (and water) and room temperature should etch ITO at a rate of at
least 100A/min.  The HCL mixture will be selective to glass, and also safe
to have a photoresist pattern present.

- Justin

Justin C. Borski
MEMS Program Manager
Advanced MicroSensors Inc.
[email protected]


-----Original Message-----
From: Anthony [mailto:[email protected]]
Sent: Monday, February 23, 2004 8:33 AM
To: [email protected]
Subject: [email protected] - Email found in subject -
[mems-talk] ITO Etch selective to glass


I am looking for an etch that will remove Indium Tin Oxide (ITO) on a glass
lens without damage to the lens.  The ITO will need to be patterned. What
would be the best approach to do this?

Anthony Marrs
Intellite
[email protected]



_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

**********************AMS CONFIDENTIAL AND PROPRIETARY
INFORMATION*****************************
This e-mail communication and any attachments are confidential and intended only
for the use of the designated recipients named above.



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Nano-Master, Inc.