Hiroaki,

I have always used sputtered Cr/Au.  Depending on glass thickness will
determine if you will get much or any under cutting.

Brent

Hiroaki SUZUKI wrote:

> Hi all
>
> Please allow me to ask one simple question. it might be in the past
> discussion...
> What is the best mask material for the glass etching with concentrated HF?
>
> Hiroaki
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
garber.vcf (text/x-vcard, 344 bytes)
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
University Wafer
MEMStaff Inc.