Ed,

Here's a quick model of reflectance vs. thickness of silver on BK7. Hope
this is of some use.

http://www.rockisland.com/~dgrove/Ag_Reflectance.doc

Dave

A good politician is like a good football coach. He has to be smart enough
to do a good job but dumb enough to think it matters.

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of
Edward Keough
Sent: Thursday, February 26, 2004 12:27 PM
To: mems-talk?
Subject: [mems-talk] Silver reflective layer

Would anyone know how thin of a layer of silver can I deposit on glass
that will still reflect a 325nm UV wavelength. I've done some research,
but I can not find an absolute answer. I believe its somewhere below
300nm though.

Thank you for any suggestions,
Ed Keough

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Harrick Plasma, Inc.
Nano-Master, Inc.