MEMSnet Home: MEMS-Talk: resist on rectangular shape slides
resist on rectangular shape slides
2004-02-27
Zheng Xia
2004-02-29
PRAMOD GUPTA
2004-03-01
Christopher F. Blanford
2004-03-02
M.Hornung
2004-03-03
Brubaker Chad
2004-03-04
Reuter, Markus
resist on rectangular shape slides
PRAMOD GUPTA
2004-02-29
Zheng

Take a 4" Si wafer and mount your rectangular glass piece in center of the
wafer. Mount the wafer on the spin coating chuck, and keep on dispensing the PR
only in the center of the glass piece until PR covers almost entire area of the
glass piece. Rest of the processing steps like spinning, RPM etc are same. If
you have thick glass piece, then you have to try circular Aluminum fixture
instead if Si wafer.

Good luck

(Pramod Gupta)

Zheng Xia  wrote:
Hi,

Does anyone have suggestion on how to apply uniform resist on
rectangular shape glass slides (1 x 3 inch)? I tried to spin them with
full coverage of resist on slides, but the result is not good. Resist
sometimes cannot reach corners, and it shows certain interference
pattern under light, indicating the unevenness of resist thickness.
Thank you.

Best,

-------------------------
XIA, ZHENG
Microfluidics and BioMEMS Lab
Interdisciplinary Microsystems Group
Department of Mechanical and Aerospace Engineering
University of Florida
-------------------------


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

(Pramod Gupta)

20800 Valley Green Dr., # 445

Cupertino, CA 95014

Phone: (408) 253-1646
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Addison Engineering