Have you tried heating the nanostrip/pirana etch up? That will reduce
the viscosity.

-Mike


>>> [email protected] 2/27/2004 4:43:45 PM >>>
Hi!
   I had to bond a pair of wafers using OCG thick resist. Deep RIE was
done to etch holes on the top wafer. Now that etching is done, I am
unable to separate the wafers. I have tried nanostrip & WNRD to remove
OCG. But no success so far. Any helpful suggestions would be
appreciated.


---------------------------------
Do you Yahoo!?
Get better spam protection with Yahoo! Mail
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk

Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Harrick Plasma, Inc.