MEMSnet Home: MEMS-Talk: Other rubber material instead of PDMS inMicrofabrication
Other rubber material instead of PDMS inMicrofabrication
2004-03-09
Michael D Martin
Other rubber material instead of PDMS inMicrofabrication
Michael D Martin
2004-03-09
You might consider a conformal parylene coating over your mold to act as
a diffusion barrier.

-Mike


>>> [email protected] 03/08/04 10:56 AM >>>
hello,all,
I am trying to cure MAA in a PDMS female mold, but the PMAA can not be
peeled off from the PDMS
mold.the reason might be the diffusion of MAA into the PDMS mold or
adhesion (bonding) of MAA to PDMS.
Id like your opinion to solve this problem with PDMS or recommend me
another kind of rubber instead
of PDMS.
your responsed would be greatly appreciated!
Chunmeng Lu
Department of Chemical Engineering
Ohio State Unversity

____________________________________________________________________
Check your SchoolEmail at http://www.CampusI.com
Find the LOWEST PRICES on books at http://www.campusi.com/BookFind !

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics