Hello everyone,

I am going to RF Sputter lead-zirconate-titanate (PZT)
onto platinized Si substrates. The problem I am having
is of Pb contamination, and so the cleanroom staff
here is very reluctant to allow any Pb inside. They
are afraid that Pb will be poisonous to users in the
clean room. Has anyone faced a similar problem before?
If so, please help me out here.

Thanks.

Abhishek Sivapurapu,
791 Atlantic Drive,
MiRC, Georgia Tech,
Atlanta, GA 30332

________________________________________________________________________
Yahoo! India Insurance Special: Be informed on the best policies, services,
tools and more.
Go to: http://in.insurance.yahoo.com/licspecial/index.html


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Addison Engineering
University Wafer