MEMSnet Home: MEMS-Talk: Si Etch Recipe with high (111) to (100) etch ratio
Si Etch Recipe with high (111) to (100) etch ratio
1997-01-15
Ken Westra
Si Etch Recipe with high (111) to (100) etch ratio
Ken Westra
1997-01-15
Hi,

   I'm looking for an anisotropic Si etch recipe that gives high
(greater than 20) (111) to (100) etch ratios. The EDP recipe that I'm
presently using gives an inconsistent ratios of 6 to 29 (with the same
bath). Unfortunately, I can't use KOH for my application, so I guess
I'm lloking at EDP or TMAH. Any suggestions would be welcome.

  Thanks

      Ken Westra
      Alberta Microelectronic Centre
      [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Tanner EDA by Mentor Graphics
The Branford Group
Mentor Graphics Corporation