MEMSnet Home: MEMS-Talk: recommends for negative resist?
recommends for negative resist?
2004-03-18
Leidong Mao
2004-03-19
Brubaker Chad
recommends for negative resist?
Leidong Mao
2004-03-18
Hi All,

     I am about to do KOH etch on <100> silicon wafer,
the feature size is about 50um. I am planning to use
silicon oxide as mask for KOH etch. Due to the mask, I
have to use negative photoresist to pattern the oxide.
Since I have no much experience in negative resist,
could you guys recommend some resist for me? The specs
are: silicon oxide ~1um, the spin-on resist should
withstand HF etching, exposure wavelength
350nm~450nm,feature size ~50um. Thanks.




__________________________________
Do you Yahoo!?
Yahoo! Mail - More reliable, more storage, less spam
http://mail.yahoo.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.