MEMSnet Home: MEMS-Talk: SU-8 5 Spinning Information
SU-8 5 Spinning Information
2004-03-24
Megan Moran
2004-03-25
Woo-Jin Chang
2004-03-24
Brubaker Chad
SU-8 5 Spinning Information
Brubaker Chad
2004-03-24
Megan,

A couple of good starts:

http://www.microchem.com/products/su_eight.htm

http://aveclafaux.freeservers.com/SU-8.html


Best Regards,

Chad Brubaker

EV Group       invent * innovate * implement
Technology - Tel: (602) 437-9492, Fax: (602)437-9435 e-mail:
[email protected], www.EVGroup.com

This message and any attachments contain confidential or privileged information,
which is intended for the named addressee(s) only. If you have received it in
error, please notify the sender immediately and then delete this e-mail. Please
note that unauthorized review, copying, disclosing, distributing or otherwise
making use of the information is strictly prohibited.


 -----Original Message-----
From:   [email protected] [mailto:mems-talk-
[email protected]]  On Behalf Of Megan Moran
Sent:   Tuesday, March 23, 2004 9:10 PM
To:     [email protected]
Subject:        [mems-talk] SU-8 5 Spinning Information

Hello,

My name is Megan and I'm a college student doing a research project
involving photo-lithography.  I need to spin layers of SU-8 5 onto silicone
dioxide.  The SU-8 layers need to be 1, 4, 5, 10 and 20 micrometers
thick.  Can anyone provide me with (or point me in the direction of)
information about spin speeds and times to get the desired thicknesses?

Also, if anyone has any suggestions as to things to avoid, the best way to
do this, baking times, etc. that would be greatly appreciated as well.

Thanks in advance for your help,

Megan
[email protected]


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMS Technology Review
Addison Engineering
Mentor Graphics Corporation