A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: photoresist as a sacrificial layer:abhiram
photoresist as a sacrificial layer:abhiram
2004-03-24
lgovinda
2004-03-29
Brubaker Chad
photoresist as a sacrificial layer:abhiram
lgovinda
2004-03-24
Hi all, my name is abhiram govindaraju and i am currently working on a
research project which involves testing of the mechanical properties at
the micron scale specimens.
i would like to know if anyone has used a photoresist layer as a
sacrificial layer to make SU-8 specimens at the micron scale, say 100 x
20 x 5 microns.

for the SU-8 specimens, releasing such small specimen is a problem as
the cantilever beam does not have enough stiffness and they start to
curl over.Si02 can't be used as a sacrificial layer as BHF would react
and effect the SU-8 structure while we use it to etch of the Si02 layer.

so i thought why not go for a very low material properties photoresist
layer which can be used as a sacrificial layer.so could any one of you
help me in finding the right material and the right etchant to remove
the sacrificial layer.

thanking you.

regards
abhiram.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.