Hi,

I was wondering if someone has done electrophoretic depostion of PZT. I need
to deposit a pretty thick PZT film as a piezoelectric actuator. I did some
literature research and it seems that electrophoretic deposition is the best
and fastest way to get a thick PZT film. Would you please give me some
advices or tips about the process? Thanks!




Best Regards,


Qing Yao
___________________
M&IE @ UIUC



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Mentor Graphics Corporation
Nano-Master, Inc.