MEMSnet Home: MEMS-Talk: SF6 isotropic etch
SF6 isotropic etch
2004-04-02
Qing Yao
2004-04-02
Brent Garber (2 parts)
2004-04-05
Marc Straub
2004-04-06
Kirt Williams
2004-04-02
Bill Moffat
SF6 isotropic etch
Qing Yao
2004-04-02
Hi,


I need to do SF6 isotropic dry etch of single crystal Si. I was wondering if
Silicon Nitride and Silicon Dioxide will also be etched in this process. If
so, does SF6 has good selectivity to them? I heard that people can use
Silicon Nitride or Silicon Dioxide as mask in BOSCH process (DRIE). So I
guess SF6 does have good selectivity to them. But I am not sure. Please let
me know if you have any information about this. Thanks!


Best Regards,


Qing Yao
___________________
M&IE @ UIUC



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
University Wafer
Tanner EDA by Mentor Graphics
Addison Engineering