MEMSnet Home: MEMS-Talk: wet etch of Al
wet etch of Al
2004-04-02
Zannitto, Peter J.
2004-04-02
Xiaoshan Zhu
2004-04-15
hare krishna
2004-04-02
Greg Miller
2004-04-02
William Lanford-Crick
2004-04-09
[email protected]
wet etch of Al
Xiaoshan Zhu
2004-04-02
Why not to use lift-off if you can reduce the Al thickness to ~100nm.

----- Original Message -----
From: "Zannitto, Peter J." 
To: 
Sent: Friday, April 02, 2004 12:23 AM
Subject: [mems-talk] wet etch of Al


>
> My structure consists of 250nm PMMA / 700nm of Al / 1um SiO2.
>
> I have done e-beam lith on the PMMA layer and developed.  I now want to
etch the Al down to the SiO2.
>
> Can anyone recommend an Al etchant that should be used in these
circumstances?  The selectivity of the etch between the Al and the PMMA
should be as high as possible.
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
The Branford Group
Addison Engineering