MEMSnet Home: MEMS-Talk: Problem with aluminium sputtering
Problem with aluminium sputtering
2004-04-05
Tomi Meilahti
2004-04-05
adnan merhaba
2004-04-05
Ravi Mullapudi
2004-04-06
Greg Chance
Light Boron diffusion in silicon
2004-04-06
Dau Thanh Van
2004-04-06
Shane Arthur McColman
2004-04-06
Mark Wendman
2004-04-07
Roger Brennan
2004-04-05
Gary
Problem with aluminium sputtering
adnan merhaba
2004-04-05
hello tomi,

what power are you using? is it RF or DC?
One possible reason I can think of is
contamination/oxidation of your aluminum target
thereby signficantly reducing your rate of sputtering.
Try burning in your target for a few minutes with
incremental power and try again.
Also if there is any leak in your sputter machine, it
will adversely effect your sputtering.

regards,
adnan merhaba


--- Tomi Meilahti  wrote:
> Hi everybody,
> We recently purchased an aluminium target for the
> companys rather old Leybold-Heraeus (model Z 400 I
> think) sputtering system. The problem is I can´t
> find working sputtering parameters for it. Either
> there is no aluminium coating on the test wafer at
> all or then the coating is of very dark colour. The
> process looks OK when I look through the small
> windows on the chamber walls. I´ve tried varying
> sputtering pressure and voltage. Any ideas or
> suggestions would be greatly appreciated.
> Best regards
> Tomi Meilahti
> Metorex International Oy
> Nihtisillankuja 5
> 02631 Espoo
> Puh: 09 32941316
> Fax: 09 32941301
> E-mail: [email protected]
> _______________________________________________
> [email protected] mailing list: to unsubscribe
> or change your list
> options, visit
>
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS
> processing services.
> Visit us at http://www.memsnet.org/


__________________________________
Do you Yahoo!?
Yahoo! Small Business $15K Web Design Giveaway
http://promotions.yahoo.com/design_giveaway/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
The Branford Group
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation